Capacity range and applicable processes:

- Up to 3000 kg/hr depending upon temperature and process
- Austempering (with subsequent bainite transformation)
- Austenitising
- Carbonitriding (restrictions apply)
- Gas carburising (restrictions apply)
- Hardening
- Tempering
- Combined with quenching in:
Salt (150 - 400°C)
Hot oil (100 - 250°C)
Oil (40 - 100°C)
Polymer (30 - 50°C)
Water (30 - 70°C)

Further Information on Processes >