Capacity range and applicable processes:
|
| - |
Up to 500 kg/hr depending upon temperature and process |
| - |
Austempering (with subsequent bainite transformation) |
| - |
Austenitising |
| - |
Carbonitriding |
| - |
Gas carburising |
| - |
Hardening |
| - |
Solution annealing |
| - |
Combined with quenching in:
Salt (150 - 400°C
Hot oil (100 - 250°C)
Oil (40 - 100°C)
Polymer (30 - 50°C)
Water (30 - 70°C) |