Capacity range and applicable processes:
|
| - |
Up to 1200 kg/hr depending upon temperature and process |
| - |
Austempering (with subsequent bainite transformation) |
| - |
Austenitising |
| - |
Carbonitriding |
| - |
Gas carburising |
| - |
Hardening |
| - |
Nitrocarburising |
| - |
Solution annealing |
| - |
Tempering |
| - |
Combined with quenching in:
- Salt (150 - 400°C)
- Hot oil (100 - 250°C)
- Oil (40 - 100°C)
- Polymer (30 - 50°C)
- Water (30 - 70°C) |
Further Information on Processes >
|