Capacity range and applicable processes:

-

Up to 500 kg/hr depending upon temperature and process

-

Austempering (with subsequent bainite transformation)

-

Austenitising

-

Blueing

- Carbonitriding
- Gas carburising
- Hardening
- Nitrocarburising
- Solution annealing
- Spheroidize annealing
- Tempering
- Combined with quenching in:
- Salt (150 - 400°C)
- Hot oil (100 - 250°C)
- Oil (40 - 100°C)
- Polymer (30 - 50°C)
- Water (30 - 70°C)

Further Information on Processes >